  • Nīnau 1: Pehea e pili ai ka ikaika o ka pōhaku wili i ka hoʻololi kala o ka ʻili kaʻa?

    Pane:
    Wahi a ka ʻatikala, i ka piʻi ʻana o ka ikaika o ka pōhaku wili, hoʻololi ke kala o ka ʻili kaʻa honua mai ka uliuli a me ka melemele-ʻeleʻele i ke kala kumu o ke kaʻaahi. Hōʻike kēia i nā pōhaku wili ikaika haʻahaʻa e alakaʻi i nā mahana wili kiʻekiʻe, e hopena i ke ahi kaʻaahi hou aʻe, i ʻike ʻia ma ke ʻano he loli kala.
  • Nīnau 2: Pehea e hiki ai i kekahi ke hoʻomaopopo i ke kiʻekiʻe o ke ahi mai ka hoʻololi ʻana o ke kala ma hope o ka wili?

    Pane:
    Ua ʻōlelo ka ʻatikala i ka wā ma lalo o 471 ° C ka mahana wili, ʻike ʻia ka ʻili o ke kaʻaahi i kona kala maʻamau; ma waena o 471-600 ° C, hōʻike ke kaʻaahi i nā ahi melemele māmā; a ma waena o 600-735°C, hōʻike ka ʻili o ke kaʻaahi i ke ahi polū. No laila, hiki i kekahi ke hoʻomaopopo i ke kiʻekiʻe o ke ahi o ke kaʻaahi ma ka nānā ʻana i nā loli kala ma ka ʻili o ke kaʻaahi ma hope o ka wili ʻana.
  • Nīnau 3: He aha ka hopena o ka wili pōhaku ikaika i ke degere oxidation o ka ʻili kaʻa?

    Pane:
    Hōʻike ka hopena o ka loiloi EDS ma ka ʻatikala me ka hoʻonui ʻana i ka ikaika o ka pōhaku wili, e emi ana ka ʻike o nā mea oxygen ma ka ʻili o ke kaʻaahi, e hōʻike ana i ka emi ʻana o ke degere oxidation o ka ʻili kaʻa. Kūlike kēia me ke ʻano o ka hoʻololi ʻana o ka waihoʻoluʻu ma ka ʻili o ke kaʻaahi, e hōʻike ana i ka ikaika haʻahaʻa o ka wili pōhaku e alakaʻi i ka oxidation koʻikoʻi.
  • Nīnau 4: No ke aha i ʻoi aku ka kiʻekiʻe o ka oxygen ma ka ʻili o lalo o ka ʻōpala wili ma mua o ka ʻili o ke kaʻa?

    Pane:
    Hōʻike ka ʻatikala i ka wā o ka hoʻokumu ʻia ʻana o ka ʻōpala, hiki ke hoʻololi i ka plastic a hana ʻia ka wela ma muli o ke kaomi ʻana o nā abrasives; i ka wā o ke kahe ʻana o ka ʻōpala, ʻānai ka ʻili lalo o ka ʻōpala i ka ʻili mua o ka ʻōpala a hoʻohua i ka wela. No laila, ʻo ka hopena hui ʻana o ka debris deformation a me ka frictional wela e alakaʻi i kahi kiʻekiʻe o ka oxidation ma ka ʻili o lalo o ka ʻōpala, ka hopena i kahi kiʻekiʻe o nā mea oxygen.
  • Nīnau 5: Pehea e hōʻike ai ka loiloi XPS i ke kūlana kemika o nā huahana oxidation ma ka ʻili kaʻa?

    Pane:
    Hōʻike nā hualoaʻa hōʻike XPS ma ka ʻatikala aia nā piko C1, O1, a me Fe2p ma ka ʻili o ke kaʻaahi ma hope o ka wili ʻana, a ke emi nei ka pākēneka o nā ʻātoma O me ke degere o ke ahi ma ka ʻili o ke kaʻaahi. Ma o ka nānā ʻana i ka XPS, hiki ke hoʻoholo ʻia ʻo nā huahana oxidation nui ma ka ʻili o ke kaʻaahi he hao hao, ʻo ia hoʻi ʻo Fe2O3 a me FeO, a i ka emi ʻana o ke degere o ke kuni, piʻi ka ʻike o Fe2+ i ka emi ʻana o ka ʻike o Fe3+.
  • Nīnau 6: Pehea e hiki ai i kekahi ke hoʻoholo i ke kiʻekiʻe o ke ahi o ka ʻili o ke kaʻaahi mai nā hopena o ka loiloi XPS?

    Pane:
    Wahi a ka ʻatikala, hōʻike ʻia nā pākēneka wahi kiʻekiʻe ma ka Fe2p narrow spectrum mai ka hōʻike XPS mai RGS-10 a i RGS-15, ka piʻi ʻana o nā pākēneka kiʻekiʻe o Fe2 + 2p3/2 a me Fe2 + 2p1/2 a ʻo ka emi ʻana o nā pākēneka wahi kiʻekiʻe o Fe3 + 2p3/2 a me Fe3 + 2p1/2. Hōʻike kēia i ka emi ʻana o ka wela o ka ʻili ma ke kaʻaahi, e piʻi ana ka ʻike o Fe2+ i nā huahana oxidation o ka ʻili, ʻoiai ke emi nei ka ʻike o Fe3+. No laila, hiki i kekahi ke hoʻoholo i ke kiʻekiʻe o ka wela o ke kaʻaahi mai ka hoʻololi like ʻana o Fe2+ a me Fe3+ i nā hopena loiloi XPS.
  • Q1: He aha ka ʻenehana High-speed Grinding (HSG)?

    A: ʻO ka ʻenehana High-speed Grinding (HSG) kahi ʻenehana kiʻekiʻe i hoʻohana ʻia no ka mālama ʻana i ke kaʻaahi kiʻekiʻe. Hoʻohana ʻia ia ma o nā neʻe huila sliding-rolling composite, i alakaʻi ʻia e nā mana paʻakikī ma waena o nā huila wili a me ka ʻili o ke kaʻaahi. Hiki i kēia ʻenehana ke hoʻoneʻe i nā mea a me ka hoʻomaʻamaʻa ponoʻī ʻana, hāʻawi i ka wikiwiki o ka wili ʻana (60-80 km/h) a me ka hoʻohaʻahaʻa ʻana i nā puka makani i hoʻohālikelike ʻia me ka wili maʻamau.
  • Nīnau 2: Pehea ka hopena o ka Sliding-Rolling Ratio (SRR) i ka hana wili?

    A: ʻO ka Sliding-Rolling Ratio (SRR), ʻo ia ka lakio o ka māmā holo ʻana i ka wikiwiki o ka holo ʻana, e hoʻoikaika nui i ka hana wili. Ke piʻi aʻe ka huina hoʻopili a me ka ukana wili, piʻi ka SRR, e hōʻike ana i nā loli i ka neʻe hui ʻana o nā hui wili. ʻO ka hoʻololi ʻana mai ka neʻe ʻana i ka ʻōwili ʻia i ke kaulike ma waena o ka hoʻoheheʻe ʻana a me ka ʻōwili ʻana e hoʻomaikaʻi nui i nā hopena wili.
  • Q3: No ke aha e pono ai ka hoʻonui ʻana i ke kihi pili?

    A: ʻO ka hoʻonui ʻana i ke kihi pili e hoʻomaikaʻi i ka maikaʻi o ka wili a me ka maikaʻi o ka ʻili. Hōʻike nā haʻawina e loaʻa ana i kahi kihi hoʻopili 45 ° ka ʻoi aku ka maikaʻi o ka wili ʻana, aʻo kahi kihi pili 60 ° e hāʻawi i ka maikaʻi o ka ʻili. E emi nui ana ka 'olika (Ra) i ka pi'i 'ana o ka huina pili.
  • Q4: He aha ka hopena o nā hopena hoʻohui thermo-mechanical i ka wā o ka wili?

    A: Thermo-mechanical coupling effects, me ke koʻikoʻi pili kiʻekiʻe, ka wela kiʻekiʻe, a me ka hoʻolili wikiwiki, alakaʻi i ka hoʻololi metallurgical a me ka deformation plastic ma ka ʻili o ke kaʻaahi, ka hopena i ka hoʻokumu ʻia ʻana o kahi papa etching keʻokeʻo brittle (WEL). Hiki i kēia WEL ke haʻihaʻi ma lalo o ke koʻikoʻi cyclic mai ka huila huila. Hana nā hana HSG i WEL me ka mānoanoa awelika o lalo o 8 micrometers, ʻoi aku ka lahilahi ma mua o ka WEL i hoʻoulu ʻia e ka wili ikaika (~40 micrometers).
  • Q5: Pehea e kōkua ai ka ʻeli ʻana i nā ʻōpala i ka hoʻomaopopo ʻana i nā ʻano hana wehe?

  • Q6: Pehea e pili ai ka wili a me ka ʻōwili ʻana i ka wā o ka wili?

  • Q7: Pehea e hoʻomaikaʻi ai i ka hana wili ʻana i ka hana wili?

  • Q8: He aha nā hopena kūpono o kēia noiʻi no ka mālama ʻana i ke kaʻaahi kiʻekiʻe?